Lift sling rigging company manufacture Aramid braided rope,Aramid Fiber Rope,Braided Aramid Cord,Aramid Fibre Braided Ropes 400 °C.
Aramidilla punottu köysi
Para-aramid 12-strand braid for heat, stretch and strength — 4 mm asti 24 mm, tehty tilauksesta
Meidän aramidilla punottu köysi is a 12-strand single braid made from 100 % para-aramidifilamentti. It is the rope to specify when the duty combines heat with strength: it has no melting point, it keeps working above 150 °C, and it holds far more of its strength at high temperature than nylon or polyester. Because it barely stretches under load, the load stays where it was set — which is why braided aramid cord is used for furnace and ladle work, heat-shield rigging, guy lines and high-temperature pulling, as well as for industrial lifting where a nylon köysi would be too elastic. Standard braids run from 4 mm asti 24 mm, silmukkasilmillä, sormustimet, hooks or buckles fitted at the ends.
- Works hot - ei sulamispistettä; strength falls to zero only near 455 °C, and long-term service is above 150 °C
- Matala venytys — a 70–100 GPa modulus keeps a suspended load steady instead of letting it settle or swing
- Strong for its weight — specific strength 5–6 times that of steel wire at roughly one fifth of the weight
- Leikkauksen ja hankausta kestävä — a dense 12-strand braid with a hard-wearing surface


Key Features of Our Aramid Braided Rope
Heat Resistance Where Nylon and Polyester Fail
Para-aramid does not melt and does not drip. It can be used continuously above 150 °C, retains about 75 % sitkeydestä sen jälkeen 100 tuntia klo 200 °C, and reaches zero strength only at about 455 °C. That is the reason this rope is specified for areas where ordinary synthetic rope would soften, glaze or fail — see also our korkea lämmönkestävä kiinnitysköysi.
Matala venymä, So the Load Stays Put
A 70–100 GPa tensile modulus means the rope gives very little under load. Where a nylon rope absorbs shock by stretching, an aramid braided rope is chosen for the opposite reason: a suspended load keeps its height, a tensioned line stays tensioned, and there is no stored energy to release when the load is set down.
12-Strand Single Braid
Twelve strands are braided without a core, so the rope is torque-free, round and even, and takes a splice that keeps most of the rope’s strength. The braid angle and density are controlled per batch, which is what fixes the finished diameter and the way the rope behaves in a hand, on a capstan or over a sheave.
Spliced Ends, Ei solmittu
A knot gives away a large part of the rope’s strength and becomes the weakest point. We finish aramid rope with hand-spliced eyes, thimble eyes, koukut, swivels or buckles, and whip or heat-seal the free ends so the braid cannot unravel.
Tekniset tiedot
| Tuote | Erittelyalue |
|---|---|
| Tuotteen nimi | Aramidilla punottu köysi / aramid fibre braided rope / braided aramid cord / Kevlar braided rope |
| Materiaali | 100 % para-aramidi (aromatic polyamide) multifilamentti, natural yellow |
| Rakentaminen | 12-yksisäikeinen punos (pyöristää); 8-nauha, 16-strand and double braid on request |
| Vakiohalkaisijat | 4 · 6 · 8 · 10 · 12 · 14 · 16 · 18 · 20 · 24 mm (custom range 3–32 mm) |
| Vakiopituudet | 100 m · 200 m · 500 m coil, 1000 m spool; mikä tahansa leikkauspituus tilauksesta |
| Väri | Natural yellow · black · custom colours |
| Pinnoite / loppuun | Päällystämätön, or PU-coated for extra abrasion resistance and a locked braid |
| Työlämpötila | Continuous service above 150 °C; strength falls to zero at about 455 °C; ei sulamispistettä |
| Pidentymä | Low — chosen where a suspended load must not settle or swing |
| UV-suoja | Protective jacket or cover recommended for permanent outdoor exposure |
| Loppuviimeistely | Hand-spliced eye · thimble eye · hook · swivel · buckle; whipped or heat-sealed ends |
| Pakkaus | Kela etiketillä, spool or carton; custom label and barcode available |
| MOQ & OEM | Alhainen MOQ koetilauksille; täysi OEM – halkaisija, väri, pituus, jatkos, painettu logo, packaging |
Vakiomääritysalue — muut halkaisijat, braid constructions and lengths are produced to order.
Halkaisija ja murtolujuus
Diameter follows from the load and from what the hardware will accept. Heavier diameters carry more, stand up to abrasion for longer and are easier to grip; lighter diameters are quicker to handle and cheaper to ship.
| Halkaisija | Noin. paino (g/m) | Tyypillinen murtolujuus | Reference working load at 5:1 |
|---|---|---|---|
| 4 mm | ≈ 11 | ≈ 15 kN (1.5 t) | ≈ 3.0 kN |
| 6 mm | ≈ 24 | ≈ 34 kN (3.5 t) | ≈ 6.8 kN |
| 8 mm | ≈ 43 | ≈ 60 kN (6.1 t) | ≈ 12.0 kN |
| 10 mm | ≈ 68 | ≈ 94 kN (9.6 t) | ≈ 18.8 kN |
| 12 mm | ≈ 97 | ≈ 135 kN (13.8 t) | ≈ 27.0 kN |
| 14 mm | ≈ 132 | ≈ 185 kN (18.9 t) | ≈ 37.0 kN |
| 16 mm | ≈ 173 | ≈ 240 kN (24.5 t) | ≈ 48.0 kN |
| 18 mm | ≈ 219 | ≈ 305 kN (31.1 t) | ≈ 61.0 kN |
| 20 mm | ≈ 270 | ≈ 377 kN (38.4 t) | ≈ 75.4 kN |
| 24 mm | ≈ 389 | ≈ 540 kN (55.0 t) | ≈ 108.0 kN |
Typical reference values for standard 12-strand aramid braid. Breaking strength and working load are confirmed by the test certificate issued for your batch — always work from that figure, not from this table.
Material Properties of Para-Aramid
| Omaisuus | Typical value |
|---|---|
| Density | 1.43 – 1.47 g/cm³ (para-aramidifilamentti, grade dependent) |
| Specific strength | 5 – 6 × that of steel wire, at roughly one fifth of the weight |
| Tensile modulus | 70 – 100 GPa at room temperature |
| Glass transition temperature | 320 – 380 °C |
| Strength retention | Noin 75 % after 100 tuntia klo 200 °C |
| Zero-strength temperature | Noin 455 °C |
| Sulamispiste | None — the fibre decomposes rather than melting (from about 500 °C) |
| Rajoittava happiindeksi | 25 – 29 (flame retardant, itsestään sammuva) |
| Moisture regain | 4.0 – 7.0 %, grade dependent (Kevlar 29 ≈ 7.0 %, Kevlar 49 ≈ 4.0 %) |
| Kemiallinen kestävyys | Good against most organic solvents; degraded by strong acids and alkalis, especially hot and concentrated |
Typical published values for para-aramid filament; confirm against the yarn datasheet used for your order.

Lämpö, Chemical and UV Behaviour
- Lämpö - ei sulamispistettä; the fibre decomposes from about 500 °C and reaches zero strength near 455 °C. Continuous service is above 150 °C.
- Kemikaalit — resistant to most organic solvents, but degraded by strong acids and alkalis, especially when hot and concentrated.
- UV — for permanent outdoor exposure, ask about a protective jacket or covered construction rather than leaving the braid bare.

Sovellukset
- Furnace, ladle and foundry rigging where radiant heat is present
- Heat shields, insulation blankets and refractory handling
- Guy lines, static lines and high-temperature pulling
- Industrial lifting and tensioning where the load must not settle
- Utility and winch duty, including the heavier forms of hyötykäyttöinen vinssijohto
- Cut-resistant cordage for slings and lanyards, alongside vetämällä köyttä ja kiipeilyköysi

Räätälöinti ja OEM-palvelu
- Halkaisija — 4–24 mm standard, 3–32 mm on request
- Rakentaminen — 12-strand single braid, tai 8-säikeinen, 16-strand and double braid
- Päättyy — spliced eye, sormustimen silmä, koukku, swivel, solki, or plain cut ends
- Pituus — any cut length; 100 m, 200 m ja 500 m keloja, 1000 m keloja
- Finishing — PU coating, väri, mid-rope marking, painettu etiketti, vähittäiskaupan pakkaus
- Täydentäviä kohteita — nauhahihna, pyöreä hihna ja turvavaljaat supplied as matched sets
Laadunvalvonta
Each batch is checked on diameter, lineaarinen tiheys, braid density and end finish, and sampled for breaking strength. We have manufactured rope and webbing for industrial, safety and sports customers for close to three decades. Pyydettäessä toimitamme lankatodistuksen, the batch test report and a sample length for you to handle and test before volume production begins.
Usein kysytyt kysymykset
What temperature can aramid braided rope take?
There is no melting point. Long-term service is above 150 °C, it keeps roughly 75 % sitkeydestä sen jälkeen 100 tuntia klo 200 °C, and its strength approaches zero at about 455 °C. Tell us the working temperature and for how long, and we will confirm the construction and whether a heat-resistant cover is needed.
Aramid braided rope or nylon rope — which one do I need?
Choose aramid for heat and low stretch; choose nylon where shock absorption and elasticity matter more than stability. If both heat and shock are present, tell us the duty rather than a fibre, and we will recommend the construction that suits it.
Can the ends be spliced?
Kyllä. A 12-strand single braid takes a hand-spliced eye that keeps most of the rope’s strength, and thimbles, koukut, swivels and buckles can be fitted to the eye. Valmis pää lyhentää käyttökelpoista pituutta, so allow for it when you order.
Do you supply kevlar braided cord in small quantities?
Kyllä. We keep the minimum order low for trial orders and will send a sample length to handle and test before volume production. Lähetä halkaisija, pituus, the working temperature and the end finish you need.
Request a Quote for Aramid Braided Rope
Lähetä meille halkaisija, pituus, the working temperature and how the rope is loaded, sekä kaikki markkinasi vaatimat merkinnät tai sertifioinnit. Our team will come back with a specification, a sample length and a factory-direct price.
Ota yhteyttä: Lift Sling Rigging Co., Ltd — puhelin ja WeChat 18066002268, sähköposti 702461526@qq.com, Lifuten teollisuuspuisto, Taizhoun kaupunki, Jiangsun maakunta, Kiina. HS koodi 630790.